Introduction of Morn heat soaked glass.
Architectural Toughened glass spontaneous breakage (about 3‰) without warning due to the expansion of nickel sulfide inclusions(NiS) present within float glass, it is inherent potential risks of toughened glass.
Learn more about tempered glass self explosion:Tempered glass and Nis
Heat soaking test is good solution to test the toughened glass and reduce the probability of self-exploded and ensure quality,the shattering proof process is used for high requirement projects.
Self-exploded glass
Production capability:
| Glass | Thickness | Min Size | Max Size |
| Heat Soaked Glass | 2.5-19mm | 300*300mm | 10000*3300mm |